Grade En58A
Corresponding Standard BS 970-1955
Wrought steels in the form of bars, billets and forgings up to 6 in. ruling section for automobile and general engineering purpose
Classification Austenitic Stainless Steel
En58A Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - 0.2 - - - 17 7 Ni+Cr≥25
Maximum Value 0.16 - 2 0.045 0.045 20 10
En58A Mechanical Properties
diameter or width across flats
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
Bar, square bloom, forging; d≤152.4 Heat Treatment ≥540 ≥185 ≥30 ≥68
• d-diameter or width across flats/mm
• The unit conversion for strength is based on: 1tons/sq.in=15.44N/mm2
• The unit conversion for impact energy absorption is based on: 1ft.lb=1.3558J
En58A Corresponding Standards(Same grade name, different standards)