USA UNS N08925
Corresponding Standard ASTM B649-2021
Ni-Fe-Cr-Mo-Cu-N Low-Carbon Alloy and Cr-Ni-Fe-N Low-Carbon Alloy Bar and Wire, Ni-Cr-Fe-Mo-N Alloy Wire, and Ni-Fe-Cr-Mo-N Alloy Bar
Classification Special Alloy Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N More
Minimum Value - - - - - 19 24 0.8 6 0.1 Fe:余量
Maximum Value 0.02 0.5 1 0.045 0.03 21 26 1.5 7 0.2
Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
All specifications Cold Finishing and Hot Finishing Annealing ≥600 ≥300 Gauge 50.8mm:
≥ 40
• For cold finished and annealed wire only, tensile strength 90 000 to 120 000 psi (620 to 830 MPa).