Grade GG-260 HB
Germany W-Nr. 0.6037
Corresponding Standard DIN 1691-1985
Cast iron with lamellar graphite (grey cast iron); properties
Classification cast Iron
GG-260 HB Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Castings; 20<t≤40 Casting State 200~275
Castings; 40<t≤80 Casting State 185~260
Approximate Comparison Table Cast Iron
China United States International Organization for Standardization Germany European Standard
GB SAE ISO DIN EN/DIN W-Nr. EN Numerical Grade
H255 H20 JL HBW255
H255
H235
H215
GG260HB 0.6037 EN-GJL-HB255 EN-JL2060
GG-260HB Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!