Grade EN-GJL-250
European Standard Steel Grade EN-JL1040
Corresponding Standard EN 1561-1997
Founding - Grey cast irons
Classification cast Iron
Density 7.2 g/cm3
EN-GJL-250 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Casting; 5<t≤300; Independent Casting Sample Casting State 250~350
Castings; 20<t≤40; casting body sample Casting State ≥210
Castings; 40<t≤80; casting body sample Casting State ≥190
Castings; 80<t≤150; casting body sample Casting State ≥170
Castings; 150<t≤300; casting body sample Casting State ≥160
New and Old Grade Replacement List
Approximate Comparison Table cast iron
China Taiwan, China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom Australia
GB CNS JIS ASTM SAE ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS Australian Standard AS
HT25-47
HT250
FC250 FC250 250/275
35
35B
40
40B
G11H20 250
JL250
GG25 0.6025 FGL250
Ft25D
EN-GJL-250 EN-JL1040 SCH25 01-25-00
0125
250
260
Grade220
Grade260
T260

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!