Grade EN-GJL-300
European Standard Steel Grade EN-JL1050
Corresponding Standard EN 1561-1997
Founding - Grey cast irons
Classification cast Iron
Density 7.25 g/cm3
EN-GJL-300 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Castings; 10<t≤300; Independent casting sample Casting State 300~400
Castings; 20<t≤40; casting body sample Casting State ≥250
Castings; 40<t≤80; casting body sample Casting State ≥220
Castings; 80<t≤150; casting body sample Casting State ≥210
Castings; 150<t≤300; casting body sample Casting State ≥190
New and Old Grade Replacement List
Approximate Comparison Table cast iron
China Taiwan, China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom Australia
GB CNS JIS ASTM SAE ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS Australian Standard AS
HT3-54
HT300
FC300 FC300 300/325
40B
45/50
45B
G13H22 300
JL300
GG30 0.6030 FGL300
Ft30D
EN-GJL-300 EN-JL1050 SCH30 01-30-00
0130
300
Grade300
T300

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!