Grade ERW 1 620-460 Cat2
Corresponding Standard BS 3059-2-1990
Steel Boiler and Superheater Tubes - Part 2. Specification For Carbon, Alloy and Austenitic Stainlesssteel Tubes with Specified Elevated Temperature Properties
Classification Alloy Steel
Density 7.85 g/cm3
ERW 1 620-460 Cat2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni * Cu * Mo Al Sn *
Minimum Value 0.1 0.1 0.4 - - 0.7 - - 0.45 - -
Maximum Value 0.15 0.35 0.7 0.03 0.03 1.1 0.3 0.25 0.65 0.02 0.03
ERW 1 620-460 Cat2 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe Room Temperature 460~610 ≥180 ≥22
Steel pipe Normalizing Rp0.2≥187
Steel pipe Normalizing Rp0.2≥180
Steel pipe Normalizing Rp0.2≥174
Steel pipe Normalizing Rp0.2≥169
Steel pipe Normalizing Rp0.2≥166

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!