Grade S2 629-470 Cat1
Corresponding Standard BS 3059-2-1990
Steel Boiler and Superheater Tubes - Part 2. Specification For Carbon, Alloy and Austenitic Stainlesssteel Tubes with Specified Elevated Temperature Properties
Classification Alloy Steel
Density 7.73 g/cm3
S2 629-470 Cat1 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni * Cu * Mo Al Sn *
Minimum Value - 0.25 0.3 - - 8 - - 0.9 - -
Maximum Value 0.15 1 0.6 0.03 0.03 10 0.3 0.25 1.1 0.02 0.03
S2 629-470 Cat1 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe Room Temperature 470~620 ≥185 ≥20
Steel pipe Annealing Rp0.2≥121
Steel pipe Annealing Rp0.2≥117
Steel pipe Annealing Rp0.2≥115
Steel pipe Annealing Rp0.2≥112

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!