Grade S1 762 Cat2
Corresponding Standard BS 3059-2-1990
Steel boiler and superheater tubes - Part 2. Specification for carbon, alloy and austenitic stainlesssteel tubes with specified elevated temperature properties
Classification Alloy Steel
Density 7.73 g/cm3
S1 762 Cat2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo V
Minimum Value 0.17 - - - - 10 0.3 - 0.8 0.25
Maximum Value 0.23 0.5 1 0.03 0.03 12.5 0.8 0.25 1.2 0.35
S1 762 Cat2 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe Room Temperature 720~870 ≥470 ≥15
Steel pipe Normalizing + Tempering Rp0.2≥345
Steel pipe Normalizing + Tempering Rp0.2≥337
Steel pipe Normalizing + Tempering Rp0.2≥324
Steel pipe Normalizing + Tempering Rp0.2≥296