Grade CFS 316S52 Cat2
Corresponding Standard BS 3059-2-1990
Steel boiler and superheater tubes - Part 2. Specification for carbon, alloy and austenitic stainlesssteel tubes with specified elevated temperature properties
Classification Ferritic Stainless Steel
Density 7.97 g/cm3
CFS 316S52 Cat2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo B
Minimum Value 0.04 - - - - 16.5 10.5 2 0.0015
Maximum Value 0.1 1 2 0.04 0.03 18.5 13.5 2.5 0.006
CFS 316S52 Cat2 Mechanical Properties
condition Test Temperature Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe Room Temperature 510~710 ≥240 ≥35
Steel pipe Solid Solution Treatment Rp1.0≥150
Steel pipe Solid Solution Treatment Rp1.0≥143
Steel pipe Solid Solution Treatment Rp1.0≥137
Steel pipe Solid Solution Treatment Rp1.0≥133
Steel pipe Solid Solution Treatment Rp1.0≥129
Steel pipe Solid Solution Treatment Rp1.0≥125
Steel pipe Solid Solution Treatment Rp1.0≥121
Steel pipe Solid Solution Treatment Rp1.0≥119
Steel pipe Solid Solution Treatment Rp1.0≥116

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!