Grade 4Cr17Ni2
Corresponding Standard Q/RP 007-2018
Stainless Steel Wire Rod
Classification Martensitic Stainless Steel
4Cr17Ni2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.11 - - - - 16 1.5
Maximum Value 0.17 0.8 0.8 0.04 0.03 18 2.5
4Cr17Ni2 Mechanical Properties
delivery condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Annealing + Pickling 650°C~700°C Air Cooling ≤850 - - ≤285