Grade 35XM
Corresponding Standard GOST 4543-1971
Alloyed Construction Steel Specifications
Classification Alloy Steel
35XM Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value 0.32 0.17 0.4 - - 0.8 - - 0.15
Maximum Value 0.4 0.37 0.7 0.035 0.035 1.1 0.3 0.3 0.25
• The letter A at the end of the grade stands for “high quality steel”. Character III means “Extra high quality steel”. For example, quality steel -30XΓC; High quality steel -30XΓCA; Extra high quality steel -30X ΓC-Ⅲ and 30XΓCA-Ⅲ.
35XM Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Impact Energy Absorption
KV2
J
Bars, forgings; d=25 Quenching and Tempering ≥930 ≥835 ≥12 ≥45 KCU
≥78
• d=circle diameter or quadrate side,unit mm
• Mechanical properties suitable for diameter or thickness less than or equal to 80mm, other sizes of mechanical properties requirements see the standard original.
• The impact test shall comply with GOST 9454-78.
• If the yield phenomenon is not obvious and the yield stress σT(i.e., σs) cannot be determined, the yield limit σ0.2(i.e., Rp0.2) is allowed.
• Allowable deviation of heat treatment temperature: quenching ±15°C; Low temperature tempering ±30°C; High temperature tempering ±50°C
Approximate Comparison Table Structural Alloy Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS14 BS EN/BS
35CrMo
35CrMoV
A30352
A31352
SCM435 SCM435
SCM435H
SCM435 4135 G41350 34CrMo4 34CrMo4 1.7220 35CD4 34CrMo4 1.7220 35XM
35ХМФ
2234 708A37
CDS13

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!