Grade X39CrMo17-1
European Standard Steel Grade 1.4122
Corresponding Standard EN 10088-2-2005
Stainless steels – Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
X39CrMo17-1 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.33 - - - - 15.5 - 0.8
Maximum Value 0.45 1 1.5 0.04 0.015 17.5 1 1.3
ⓑParticular ranges of sulphur content may provide improvement of particular properties. For machinability a controlled sulphur content of 0.015 % to 0.030% is recommended and permitted. For weldability, a controlled sulphur content of 0.008 % to 0.030 % is recommended and permitted. For polishability, a controlled sulphur content of 0.015 % max is recommended.
X39CrMo17-1 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Impact Energy Absorption
KV2
J
Steel +QT750 750~950 550 14~20
Approximate Comparison Table Martensitic Stainless Steel
International Organization for Standardization European Standard
ISO Numerical Grade EN Numerical Grade
X39CrMo17-1 4122-434-09-I X39CrMo17-1 1.4122

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!