Grade NA 15(H)
Corresponding Standard BS 3076-1989
Specification for Nickel and Nickel Alloys: Bar
Classification Nickel and Nickel Alloys
NA 15(H) Chemical Element Composition Content (%)
Component C Si Mn S Cr Ni * Cu Ti Al More
Minimum Value 0.05 - - - 19 30 - 0.15 0.15 Fe: Remainder
Maximum Value 0.1 1 1.5 0.015 23 35 0.75 0.6 0.6
* Including not more than 2% cobalt
NA 15(H) Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Bar (Round, Square, Rectangular, and Hexagonal); All Sizes cold worked and solution treated* ≥450 ≥170 ≥30
round bars; all size hot worked and solution treated* ≥450 ≥170 ≥30
Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany United Kingdom
GB Commercial Grade UNS DIN EN/DIN W-Nr. BS EN/BS
NS112 Incoloy 800H N08810 X5NiCrAlTi31-20 1.4958 NA15(H)