Grade 07Cr25Ni20
China ISC S31009
Old Grade
Corresponding Standard GB /T 20878-2024
Stainless Steels - Designation and Chemical Composition
Classification Austenitic Stainless Steel
Density 7.98 g/cm3
07Cr25Ni20 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.04 - - - - 24 19
Maximum Value 0.1 0.75 2 0.03 0.015 26 22
Approximate Comparison Table Seamless Steel Tubes and Pipes for High Pressure Boiler
China United States
GB ISC ASTM/AISI
07Cr25Ni21 S31009 SA-213 TP310H

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!