Grade C30EC
Corresponding Standard ISO 4954-1-2024
Steels for Cold Heading and Cold Extruding - Technical Delivery Conditions - Part1: Non-Alloy and Alloy Steels
Classification Carbon Steel
C30EC Chemical Element Composition Content (%)
Component C Si Mn P S Cu
Minimum Value 0.27 - 0.5 - - -
Maximum Value 0.33 0.3 0.8 0.025 0.025 0.25
C30EC Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
10<d≤40 +AC or
+AC+PE
≤590 -
2≤d≤40 +AR+C+AC+LC ≤620 ≥55
5<d≤40 +AC+C ≤620 ≥55
①+AR=as hot-rolled;+AR or +PE=as hot-rolled or peeled;+AR+C=as hot-rolled+cold drawn;+AR+C+AC=as hot-rolled+cold drawn+spheroidized;+AR+C+AC+LC=as hot-rolled+cold drawn+spheroidized+skin passed;+AC= spheroidized ;+AC or +AC+PE=spheroidized or spheroidized+peeled;+AC+C=spheroidized +cold drawn;+FP=treated to ferrite-pearlite structure and hardness range;+AC+C+AC=spheroidized +cold drawn + spheroidized;+AC+C+AC+LC=spheroidized +cold drawn + spheroidized + skin passed
• Mechanical properties of cold heading and cold extruding steels for quenching and tempering
Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
Japan International Organization for Standardization European Standard
JIS ISO EN
SWRCH30K C30EC C30EC
C30EC Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!