Grade C35EC
Corresponding Standard ISO 4954-1-2024
Steels for cold heading and cold extruding - Technical delivery conditions - Part1: Non-alloy and alloy steels
Classification Carbon Steel
C35EC Chemical Element Composition Content (%)
Component C Si Mn P S Cu
Minimum Value 0.32 - 0.5 - - -
Maximum Value 0.39 0.3 0.8 0.025 0.025 0.25
C35EC Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or
+AC+PE
≤560 ≥60
2≤d≤5 +AR+C+AC ≤550 ≥62
5<d≤40 ≤540 ≥62
2≤d≤5 +AR+C+AC+LC ≤590 ≥60
5<d≤40 ≤580 ≥60
5<d≤10 +AC+C ≤670 -
10<d≤40 ≤660 -
①+AR=as hot-rolled;+AR or +PE=as hot-rolled or peeled;+AR+C=as hot-rolled+cold drawn;+AR+C+AC=as hot-rolled+cold drawn+spheroidized;+AR+C+AC+LC=as hot-rolled+cold drawn+spheroidized+skin passed;+AC= spheroidized ;+AC or +AC+PE=spheroidized or spheroidized+peeled;+AC+C=spheroidized +cold drawn;+FP=treated to ferrite-pearlite structure and hardness range;+AC+C+AC=spheroidized +cold drawn + spheroidized;+AC+C+AC+LC=spheroidized +cold drawn + spheroidized + skin passed
• Mechanical properties of cold heading and cold extruding steels for quenching and tempering
1 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard Russia
ISO EN GOST
C35EC C35EC 1.1172
2 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
China Japan United States International Organization for Standardization European Standard
GB JIS ASTM ISO EN
ML38 SWRCH38K 1038 C35EC C35EC

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!