Grade 41CrS4
Corresponding Standard ISO 4954-1-2024
Steels for cold heading and cold extruding - Technical delivery conditions - Part1: Non-alloy and alloy steels
Classification Alloy Steel
41CrS4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.38 - 0.6 - 0.02 0.9 -
Maximum Value 0.45 0.3 0.9 0.025 0.04 1.2 0.25
41CrS4 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or +AC+PE ≤620 ≥58
2≤d≤5 +AC+C+AC ≤610 ≥60
5<d≤40 ≤600 ≥60
2≤d≤5 +AC+C+AC+LC ≤650 ≥58
5<d≤40 ≤640 ≥58
①+AR=as hot-rolled;+AR or +PE=as hot-rolled or peeled;+AR+C=as hot-rolled+cold drawn;+AR+C+AC=as hot-rolled+cold drawn+spheroidized;+AR+C+AC+LC=as hot-rolled+cold drawn+spheroidized+skin passed;+AC= spheroidized ;+AC or +AC+PE=spheroidized or spheroidized+peeled;+AC+C=spheroidized +cold drawn;+FP=treated to ferrite-pearlite structure and hardness range;+AC+C+AC=spheroidized +cold drawn + spheroidized;+AC+C+AC+LC=spheroidized +cold drawn + spheroidized + skin passed
1 Approximate Comparison Table
International Organization for Standardization Germany France European Standard Russia Sweden
ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS
41CrS4 41CrS4 1.7039 42C4u 41CrS4 1.7039 40KH 2245
2 Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
41CrS4 41CrS4 1.7039