Grade 25CrMo4
Corresponding Standard ISO 4954-1-2024
Steels for cold heading and cold extruding - Technical delivery conditions - Part1: Non-alloy and alloy steels
Classification Alloy Steel
25CrMo4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo
Minimum Value 0.22 - 0.6 - - 0.9 - 0.15
Maximum Value 0.29 0.3 0.9 0.025 0.025 1.2 0.25 0.3
25CrMo4 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or +AC+PE ≤580 ≥60
2≤d≤5 +AC+C+AC ≤570 ≥62
5<d≤40 ≤560 ≥62
2≤d≤5 +AC+C+AC+LC ≤610 ≥60
5<d≤40 ≤600 ≥60
①+AR=as hot-rolled;+AR or +PE=as hot-rolled or peeled;+AR+C=as hot-rolled+cold drawn;+AR+C+AC=as hot-rolled+cold drawn+spheroidized;+AR+C+AC+LC=as hot-rolled+cold drawn+spheroidized+skin passed;+AC= spheroidized ;+AC or +AC+PE=spheroidized or spheroidized+peeled;+AC+C=spheroidized +cold drawn;+FP=treated to ferrite-pearlite structure and hardness range;+AC+C+AC=spheroidized +cold drawn + spheroidized;+AC+C+AC+LC=spheroidized +cold drawn + spheroidized + skin passed
1 Approximate Comparison Table
China Japan International Organization for Standardization European Standard
GB ISC JIS ISO EN Numerical Grade
30CrMo A30302 SCM425
SCM425H
25CrMo4 25CrMo4 1.7218
2 Approximate Comparison Table structural alloy steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS SAE ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
30CrMo SCM420
SCM430
4130 25CrMo4 25CrMo4 25CD4 25CrMo4 1.7218 20KHM
30KHM
30KHMA
2225 708A25
708M25
CFS10
3 Approximate Comparison Table
Japan International Organization for Standardization European Standard
JIS ISO EN Numerical Grade
SCM425
SCM425H
25CrMo4 25CrMo4 1.7218