Grade 37CrMo4
Corresponding Standard ISO 4954-1-2024
Steels for cold heading and cold extruding - Technical delivery conditions - Part1: Non-alloy and alloy steels
Classification Alloy Steel
37CrMo4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo
Minimum Value 0.35 - 0.6 - - 0.9 - 0.15
Maximum Value 0.4 0.3 0.9 0.025 0.025 1.2 0.25 0.3
37CrMo4 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
5<d≤40 +AC or +AC+PE ≤620 ≥60
2≤d≤5 +AC+C+AC ≤610 ≥62
5<d≤40 ≤600 ≥62
2≤d≤5 +AC+C+AC+LC ≤650 ≥60
5<d≤40 ≤640 ≥60
①+AR=as hot-rolled;+AR or +PE=as hot-rolled or peeled;+AR+C=as hot-rolled+cold drawn;+AR+C+AC=as hot-rolled+cold drawn+spheroidized;+AR+C+AC+LC=as hot-rolled+cold drawn+spheroidized+skin passed;+AC= spheroidized ;+AC or +AC+PE=spheroidized or spheroidized+peeled;+AC+C=spheroidized +cold drawn;+FP=treated to ferrite-pearlite structure and hardness range;+AC+C+AC=spheroidized +cold drawn + spheroidized;+AC+C+AC+LC=spheroidized +cold drawn + spheroidized + skin passed
Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
37CrMo4 37CrMo4 1.7202
37CrMo4 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!