Grade E355
Germany W-Nr. 1.0580
Corresponding Standard DIN EN 10305-1-2003
Steel Tubes for Precision Applications – Technical Delivery Conditions – Part 1: Seamless Cold Drawn Tubes
Classification Carbon Steel
E355 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value - - - - -
Maximum Value 0.22 0.55 1.6 0.025 0.025
① Additions of Nb, Ti and V are permitted at the choice of the manufacturer. Indicate the proportion of these elements.
② For the steel grades E235, a controlled sulfur content ranging from 0.015% to 0.040% is specified to improve the machinability. It is to be adjusted by resulfurization of the steel after maximum desulfurization or alternatively by secondary metallurgical processes with a reduction of the oxygen content.
E355 Mechanical Properties
condition Mark
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Seamless steel pipe E355 +N Normalizing (+N) 490~630
≥355
≥22
Seamless steel pipe E355 +SR Cold Drawing and Stress Relief (+SR) ≥580
≥450
≥10
Seamless steel pipe E355 +A Soft Annealed (+A)** ≥450 ≥22
Seamless steel pipe E355 +LC Cold Finishing (+LC)* ≥580 ≥7
Seamless steel pipe E355 +C Cold Drawn Hardening (+C)* ≥640 ≥4
1 Approximate Comparison Table Construction Rebar
China Japan International Organization for Standardization Germany Russia
GB ISC JIS ISO DIN EN/DIN GOST
HRB335 L33350 SD345 PB300
RB300
E355 Ат400С
2 Approximate Comparison Table High-Quality Carbon Structural Steel
China United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
Q390C Gr.65 Fe590 E355
St52
St52-3
1.0060 E335
ES355
TS-47a
TU526
E355 1.0580 St6sp 1650 CEW5
CFS5
E335
ERW5NKM
ERW5NZF
E355 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!