Grade X2CrNi18-9
Germany W-Nr. 1.4307
Corresponding Standard DIN EN 10296-2-2006
Welded circular steel tubes for mechanical and general engineering purposes — Technical delivery conditions — Part 2 Stainless steel
Classification Austenitic Stainless Steel
X2CrNi18-9 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 17.5 8 -
Maximum Value 0.03 1 2 0.045 0.015 19.5 10.5 0.11
① a controlled sulfur content of 0,015% to 0,030% is specified.
X2CrNi18-9 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe: ≥470 Rp0.2:≥180
Rp1.0:≥215
l:≥40
t:≥35
◎ l=longitudinal, t=transverse
◎ Resistance to intergranular corrosiona: Yes (When tested in accordance with EN ISO3651-2)