Grade X12CrNi23-13
Germany W-Nr. 1.4833
Corresponding Standard DIN EN 10296-2-2006
Welded Circular Steel Tubes for Mechanical and General Engineering Purposes — Technical Delivery Conditions — Part 2 Stainless Steel
Classification Austenitic Stainless Steel
X12CrNi23-13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 22 12 -
Maximum Value 0.15 1 2 0.045 0.015 24 14 0.11
X12CrNi23-13 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe: ≥500 Rp0.2:≥210
Rp1.0:≥250
l:≥35;t:≥35
◎ l=longitudinal, t=transverse
◎ Elongation 20% min for wall thickness ≤35 mm after cold deformation.
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
06Cr23Ni13
(0Cr23Ni13)
S30908 309S SUS 309S STS 309S 309S S30908 X12CrNi 23-13
X6CrNi23-13
X7CrNi 23-14 1.4833 Z15CN 24-13 X12CrNi 23-13
X6CrNi23-13
1.4833
1.4950
10Х23Н13
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
06Cr23Ni13
(0Cr23Ni13)
S30908 309S SUS 309S STS 309S 309S S30908 X12CrNi 23-13 X7CrNi 23-14
X12CrNi 23-13
1.4833
1.4833
Z15CN 24-13 X12CrNi 23-13 1.4833 10Х23Н13

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!