Grade X2CrNiN18-7
European Standard Steel Grade 1.4318
Corresponding Standard EN 10296-2-2005
Welded circular steel tubes for mechanical and general engineering purposes — Technical delivery conditions — Part 2 Stainless steel
Classification Austenitic Stainless Steel
X2CrNiN18-7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 16.5 6 0.1
Maximum Value 0.03 1 2 0.045 0.015 18.5 8 0.2
X2CrNiN18-7 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe: ≥630 Rp0.2:≥330
Rp1.0:≥370
l:≥45
t:≥45
◎ l=longitudinal, t=transverse
◎ Resistance to intergranular corrosiona: Yes (When tested in accordance with EN ISO3651-2)
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS ASTM UNS ISO Numerical Grade EN Numerical Grade
S30153 SUS 301L 301LN S30153 X2CrNiN18-7 4318-301-53-I X2CrNiN18-7 1.4318
2 Approximate Comparison Table Austenitic Stainless Steel
Japan United States France European Standard
JIS ASTM NF EN/NF EN Numerical Grade
SUS301L 301LN Z3CN18-07Az X2CrNiN18-7 1.4318

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!