Grade X2CrNiMo18-14-3
European Standard Steel Grade 1.4435
Corresponding Standard EN 10296-2-2005
Welded Circular Steel Tubes for Mechanical and General Engineering Purposes — Technical Delivery Conditions — Part 2 Stainless Steel
Classification Austenitic Stainless Steel
X2CrNiMo18-14-3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 17 12.5 2.5 -
Maximum Value 0.03 1 2 0.045 0.015 19 15 3 0.11
① a controlled sulfur content of 0,015% to 0,030% is specified.
X2CrNiMo18-14-3 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe: ≥490 Rp0.2:≥190
Rp1.0:≥225
l:≥40
t:≥35
◎ l=longitudinal, t=transverse
◎ Resistance to intergranular corrosiona: Yes (When tested in accordance with EN ISO3651-2).
Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
00Cr17Ni14Mo2 SUS316L 316L
TP316L
Type19a X2CrNiMo18-14-3 Z3CND17-12-03
Z3CND18-14-03
X2CrNiMo18-14-3 1.4435 03KH17N14M3 2353 316S13
316S14

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!