Grade X1CrNiMoCuN20-18-7
European Standard Steel Grade 1.4547
Corresponding Standard EN 10296-2-2005
Welded Circular Steel Tubes for Mechanical and General Engineering Purposes — Technical Delivery Conditions — Part 2 Stainless Steel
Classification Austenitic Stainless Steel
X1CrNiMoCuN20-18-7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 19.5 17.5 0.5 6 0.18
Maximum Value 0.02 0.7 1 0.03 0.01 20.5 18.5 1 7 0.25
X1CrNiMoCuN20-18-7 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Steel pipe: ≥650 Rp0.2:≥300
Rp1.0:≥340
l:≥35
t:≥30
◎ l=longitudinal, t=transverse
◎ Resistance to intergranular corrosiona: Yes (When tested in accordance with EN ISO3651-2).
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard Sweden
GB ISC JIS ASTM UNS ISO EN Numerical Grade SS
015Cr20Ni18Mo6CuN S31252 SUS 312L S31254 S31254 X1CrNiMoN 20-18-7
X1CrNiMoCuN20-18-7
X1CrNiMoCuN 20-18-7 1.4547 254SMO
2 Approximate Comparison Table Austenitic Stainless Steel
China United States Germany European Standard Sweden
GB Commercial Grade UNS DIN EN/DIN W-Nr. EN Numerical Grade SS
254SMo 254SMO S31254 X1CrNiMoCuN20-18-7 1.4547 X1CrNiMoCuN20-18-7 1.4547 2378

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!