Grade STS 410
Other Names
Corresponding Standard KS D 3697-2002
Stainless Steel Wires for Cold Heading and Cold Forging
Classification Martensitic Stainless Steel
STS 410 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 11.5 -
Maximum Value 0.15 1 1 0.04 0.03 13.5 0.6
STS 410 Mechanical Properties
diameter or thickness
d
mm
Mark
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
0.8<d≤2 STS 410-WSB 540~740 - ≥65
2<d≤17 STS 410-WSB 460~640 ≥10 ≥65
1 Approximate Comparison Table Martensitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12Cr13
(1Cr13)
S41010 410 SUS 410 STS 410 410 S41000 X12Cr 13 4006-410-00-I X10Cr 13
X12Cr 13
1.4006
1.4006
Z12C 13
Z10C13
X12Cr 13 1.4006 12Х13
12KH13
15KH13L
2302 410S21
2 Approximate Comparison Table Martensitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
12Cr13
(1Cr13)
S41010 410 SUS 410 STS 410 410 S41000 X12Cr 13
3
(ISO 683-13-1986)
X10Cr 13 1.4006 Z12C 13 X12Cr 13 1.4006 12Х13 2302 410S21
STS410 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!