Grade С345К
Other Names
Corresponding Standard GOST 27772-2015
Rolled Metal for Steel Building Structures
Classification Alloy Steel
С345К Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Ti Al
Minimum Value - 0.17 - 0.02 - 0.5 0.3 0.3 - 0.08
Maximum Value 0.12 0.37 0.6 0.12 0.025 0.8 0.6 0.5 0.035 0.15
С345К Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
4≤t≤10 ≥470 ≥345 ≥20 -40°C:
KCU≥39J/cm2

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!