Grade С355
Other Names
Corresponding Standard GOST 27772-2015
Rolled Metal for Steel Building Structures
Classification Alloy Steel
С355 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Ti V Nb Al
Minimum Value - 0.15 1 - - - - - - - - 0.2
Maximum Value 0.14 0.8 1.8 0.025 0.025 0.3 0.3 0.3 0.035 0.08 0.06 0.06
С355 Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
8≤t≤16 ≥470 ≥355 ≥21 -20°C,-40°C:
KCV≥34J/cm2
16<t≤40 ≥470 ≥345 ≥21 -20°C,-40°C:
KCV≥34J/cm2
40<t≤60 ≥470 ≥335 ≥21 -20°C,-40°C:
KCV≥34J/cm2
60<t≤80 ≥460 ≥325 ≥21 -20°C,-40°C:
KCV≥34J/cm2
80<t≤100 ≥460 ≥315 ≥21 -20°C,-40°C:
KCV≥34J/cm2
100<t≤160 ≥460 ≥295 ≥21 -20°C,-40°C:
KCV≥34J/cm2

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!