USA UNS S44401
Corresponding Standard ASTM A493-2009(2013)
Standard Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
Classification Ferritic Stainless Steel
Properties Corrosion Resistance Good Forgability
Chemical Element Composition Content (%)
Component C Mn P S Cr Ni Mo N Ti More
Minimum Value - - - - 17.5 - 1.75 - - Ti+Cb:[0.2 + 4 x (%C + %N)]~0.8
Maximum Value 0.025 1 0.04 0.03 19.5 1 2.5 0.035 0.2
Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Wires, coils; d ≥ 2.5 Annealing ≤550
Wires, coils; d ≥ 2.5 Light Drawing ≤620

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!