Grade A571 Class 2
Corresponding Standard ASTM A 571/A571M-2001(R2023)
Standard Specification for Austenitic Ductile Iron Castings for Pressure-Containing Parts Suitable for Low-Temperature Service
Classification cast Iron
A571 Class 2 Chemical Element Composition Content (%)
Component C Si Mn P Cr Ni
Minimum Value 2.2 1.5 3.75 - - 21
Maximum Value 2.7 2.5 4.5 0.08 0.2 24
① Total carbon. For castings with sections under 6 mm, it may be desirable to adjust the carbon upwards to a maximum of 2.90 %.
② Not intentionally added.
A571 Class 2 Mechanical Properties
Tensile Strength
σb
ksi
Specified Plastic Yield Strength
Rp0.2
ksi
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≥60 ≥25 ≥25 111~171 ft·lbf
≥20