Grade A579 Grade 51
Corresponding Standard ASTM A 579-2004(R2014)
Standard Specification for Superstrength Alloy Steel Forgings
Classification Martensitic Stainless Steel
A579 Grade 51 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Al Sn
Minimum Value - - - - - 11.5 - - - - -
Maximum Value 0.15 1 1 0.025 0.025 13.5 0.75 0.5 0.5 0.05 0.05
A579 Grade 51 Mechanical Properties
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Forgings ≥1210 ≥965 ≥12 ≥45 ≥20
Forgings;Section size ≤ 50mm ≥965 Annealing
≤197

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!