Grade AlCu6BiPb
Germany W-Nr. EN AW-2011
Other Names
Old Grade
Corresponding Standard DIN EN 1301-2-2008
Aluminium and aluminium alloys-drawn wires-Part 2: Mechanical properties
Classification Aluminum and Aluminum Alloys
AlCu6BiPb Chemical Element Composition Content (%)
Component Fe Si Cu Pb Zn Bi Other Individual Other Total More
Minimum Value - - 5 0.2 - 0.2 - - Al:余量
Maximum Value 0.7 0.4 6 0.6 0.3 0.6 0.05 0.15
"Other individual elements or other totals": The chemical composition includes elements not specified in the table. Analysis should only be conducted if these elements are suspected to be present, or if routine analysis suggests that their content may exceed the prescribed limits.
AlCu6BiPb Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Drawing wire; d≤18 Solution Heat Treatment + Cold Work + Natural Aging (T3) ≥310 295 6
Drawing wire; d≤18 Solution Heat Treatment + Cold Work + Artificial Aging (T8) ≥370 310 4
Drawing wire; d≤18 Strain-Hardening - 3/8 Hard (H13) 155~255
Drawn wire; d≤10 Strain - Hardening - 4/4 Hard (H18) ≥240

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!