Grade TP 310
USA UNS S31000
Corresponding Standard ASTM A632-2019(2025)
Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service
Classification Austenitic Stainless Steel
TP 310 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 24 19
Maximum Value 0.25 1.5 2 0.045 0.03 26 22
TP 310 Mechanical Properties
diameter or thickness
d or t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
d≥3.2 or t≥0.38 ≥515 ≥205 ≥35
d<3.2 or t<0.38 / / ≥25
Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
20Cr25Ni20
(2Cr25Ni20)
S31020 SUH 310 SUH 310 STR 310 310 S31000 X15CrNi 25-21 X15CrNiSi 25-20 1.4841 Z15CNS 25-20 X15CrNi 25-20 1.4845 20Х25Н20С2 310S31