Grade HP 9-4-30
ASTM
Specification or Grade
Grade 17
Corresponding Standard ASTM A646/A646M-2024
Standard Specification for Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings
Classification Alloy Steel
HP 9-4-30 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo V Co
Minimum Value 0.29 - 0.1 - - 0.9 7 0.9 0.06 4.25
Maximum Value 0.34 0.1 0.35 0.01 0.01 1.1 8 1.1 0.12 4.75
* If any of the following elements are not specified, the following maximum limits shall apply: Nickel 0.35 %; Chromium 0.20 %; Molybdenum 0.06 %; Copper 0.35 %
HP 9-4-30 Mechanical Properties
Heat Treatment or Condition
Hardness
HBW
Annealing ≤341
Approximate Comparison Table Processing Titanium and Titanium Alloys
China Japan United States International Organization for Standardization Germany France United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF BS EN/BS
TA8-1 Class 17 Grade 17 Ti-0.05Pd(a) Ti1Pd T-Pd(a) Ti-0.05Pd(a)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!