Grade A355 Class D
Corresponding Standard ASTM A355-1989(R2012)
Steel Bars, Alloys, for Nitriding
Classification Alloy Steel
A355 Class D Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo Al
Minimum Value 0.33 0.15 0.5 - - 1 0.15 0.95
Maximum Value 0.38 0.35 0.7 0.035 0.04 1.3 0.25 1.3
A355 Class D Mechanical Properties
Heat Treatment or Condition
Hardness
HBW
quenching + temper- ing Range1:
HBW: 223~269
HRC: 19~28
HRB: 98~104
Range2:
HBW: 248~302
HRC: 24~32
HRB: 101~107