Grade 201L
USA UNS S20103
Corresponding Standard ASTM A666/A666M-2024
Standard Specification for Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar
Classification Austenitic Stainless Steel
201L Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 5.5 - - 16 3.5 -
Maximum Value 0.03 0.75 7.5 0.045 0.03 18 5.5 0.25
201L Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Annealing ≥655 ≥260 ≥40 ≤217
1/16 Hard ≥690 ≥345 ≥40
1/8 Hard ≥725 ≥380 ≥35
1/4 Hard ≥825 ≥515 ≥25
1/2 Hard ≥930 ≥690 ≥22 (thickness ≤ 0.38mm);
≥20 (thickness>0.76mm)
201L Corresponding Standards(Same grade name, different standards)