Grade C10
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Carbon Steel
Properties Carburizing Capability
C10 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.07 0.15 0.3 - -
Maximum Value 0.13 0.4 0.6 0.035 0.035
◎ A lower silicon content may be agreed upon at the time of enquiry and order; in this case, the influence on mechanical properties should be taken into account.
C10 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤5 TC ≥500 ≥400 ≥7
5<t≤10 TC ≥470 ≥360 ≥8
10<t≤16 TC ≥420 ≥310 ≥9
16<t≤25 TC ≥400 ≥285 ≥10
25<t≤40 TC ≥390 ≥270 ≥11
40<t≤100 TC ≥340 ≥170 ≥12
100<t≤160 TC Be agreed Be agreed Be agreed
Steel TC+TA,
P+TA或
G+TA
≤131

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!