Grade H08Cr19Ni10Ti
Corresponding Standard Others Q/TTPT003-2018
Stainless Steel Wire Rods for Welding
Classification Austenitic Stainless Steel
H08Cr19Ni10Ti Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N Ti
Minimum Value - 0.3 1 - - 18.5 9.1 - - - 0.5
Maximum Value 0.09 0.7 2 0.028 0.02 20 10.5 0.4 0.5 0.05 0.8
H08Cr19Ni10Ti Mechanical Properties
product Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Wire rod Offline Solution Annealing + Pickling ≤640 ≥50 ≥70
Wire rod Hot rolling + Picking ≤730 ≥50 ≥70

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!