Grade X1CrNiMoCuN20-18-7
European Standard Steel Grade 1.4547
Corresponding Standard EN 10272-2016
Stainless Steel Bars for Pressure Purposes
Classification Austenitic Stainless Steel
X1CrNiMoCuN20-18-7 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 19.5 17.5 0.5 6 0.18
Maximum Value 0.02 0.7 1 0.03 0.01 20.5 18.5 1 7 0.25
X1CrNiMoCuN20-18-7 Mechanical Properties
Diameter or thickness
d or b
mm
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≤160 650~850 Rp0.2:≥300
Rp1.0:≥340
l: ≥35 ≤260 (at 20℃):l ≥100 (at 20℃)
(at -196℃):≥60
160<d (b)≤400 650~850 Rp0.2:≥300
Rp1.0:≥340
tr: ≥30 ≤260 (at 20℃):tr ≥60
(at -196℃):≥ 60
a) Axial: l;Tangential:tr.
* The maximum HBW-values may be raised by 100 units or the tensile strength value may be raised by 200 MPa and the minimum elongation value be lowered to 20 % for bars of ≤ 35 mm thickness having a final cold deformation.
1 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard Sweden
GB ISC JIS ASTM UNS ISO EN Numerical Grade SS
015Cr20Ni18Mo6CuN S31252 SUS 312L S31254 S31254 X1CrNiMoN 20-18-7
X1CrNiMoCuN20-18-7
X1CrNiMoCuN 20-18-7 1.4547 254SMO
2 Approximate Comparison Table Austenitic Stainless Steel
China United States Germany European Standard Sweden
GB Commercial Grade UNS DIN EN/DIN W-Nr. EN Numerical Grade SS
254SMo 254SMO S31254 X1CrNiMoCuN20-18-7 1.4547 X1CrNiMoCuN20-18-7 1.4547 2378

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!