Grade S420NH
European Standard Steel Grade 1.8750
Corresponding Standard EN 10219-3-2020
Cold Formed Welded Steel Structural Hollow Sections - Part 3: Technical Delivery Conditions for High Strength and Weather Resistant Steels
Classification Alloy Steel
S420NH Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N Ti V Nb Al
Minimum Value - - 1 - - - - - - - - - - 0.02
Maximum Value 0.22 0.6 1.7 0.03 0.025 0.3 0.8 0.55 0.1 0.025 0.05 0.2 0.05 -
① If the copper content is greater than 0,30 % then the nickel content shall be at least half of the copper content.
② If sufficient N-binding elements are present, the minimum total Al content does not apply.
③ The deoxidation method is designated as follows: FF= fully killed steel containing nitrogen binding elements in amounts sufficient to bind the available nitrogen and having a fine grain structure.
S420NH Mechanical Properties
thickness
t
mm
Test Temperature Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤16 520~680 ReH: ≥420 l:≥19
t:≥17
16<t≤40 520~680 ReH: ≥400 l:≥19
t:≥17
/ l:≥40
t:≥20