Grade B316 6061
Corresponding Standard ASTM B316/B316M-2015
Standard Specification for Aluminum and Aluminum-Alloy Rivet and Cold-Heading Wire and Rods
Classification Aluminum and Aluminum Alloys
B316 6061 Chemical Element Composition Content (%)
Component Fe Si Mn Cr Cu Ti Zn Mg
Minimum Value - 0.4 - 0.04 0.15 - - 0.8
Maximum Value 0.7 0.8 0.15 0.35 0.4 0.15 0.25 1.2
B316 6061 Mechanical Properties
diameter
d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Fatigue Limit
Bending σ-1
Mpa
Elongation or Extension Rate
δ
%
1.6<d≤25 Solution Heat Treatment + Artificial Aging (T6)
≥290
Solution Heat Treatment + Artificial Aging (T6)
≥240
Shear Strength στ/Mpa
≥170
Solution Heat Treatment + Artificial Aging (T6)
≥9
d≤25 Strain-Hardening (H13)
150~210
d≤25 Annealing (O)
≤155
B3166061 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!