Grade C25
Corresponding Standard ISO 683-1-1987
Heat-Treatable Steels,alloy Steels and Free-Cutting Steels. Part 1:Direct-Hardening Unalloyed and Low-Alloyed Wrought Steel in Form of Different Black Produts
Classification Carbon Steel
C25 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.22 0.1 0.4 - -
Maximum Value 0.29 0.4 0.7 0.045 0.045
• The designations are in accordance with the system proposed by ISO/TC 17/SC 2.
• Elements not quoted should not be intentionally added to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. All reasonable precautions should be taken to prevent the addition, from scrap or other material used in manufacture, of such elements which affect the hardenability, mechanical properties and applicability.
• In the case of the grades with specified hardenability requirements (see tables 5 to 7), except for phosphorous and sulfur, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of carbon ± 0,01 % (m/m) and in all other cases the values according to table 4.
• For boron-treated steels, see ISO 4954.
• Steels with improved machinability by either lead additions or higher sulfur levels up to about 0,100 % (m/m) S (including controlled sulfide morphology) may be available on request.
C25 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
d≤16 Quenching + Tempering 550~700 ≥370 ≥19
16<d≤40 Quenching + Tempering 500~650 ≥320 ≥21
1 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China Japan International Organization for Standardization
GB JIS ISO
25 S25C C25
2 Approximate Comparison Table High-Quality Carbon Structural Steel
China Japan United States International Organization for Standardization Germany European Standard Russia Sweden United Kingdom
GB JIS SAE ISO DIN EN/DIN W-Nr. EN Numerical Grade GOST SS BS EN/BS
20 S20C
S22C
1020 C25 C22 1.0402 C22 1.0402 20 1450 070M20
3 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
International Organization for Standardization Germany European Standard Russia
ISO DIN EN/DIN EN Numerical Grade GOST
C25 C25 C25 1.0406 25
4 Approximate Comparison Table High-Quality Carbon Structural Steel
China Japan United States International Organization for Standardization France Russia United Kingdom
GB JIS ASTM/AISI ISO NF EN/NF GOST BS EN/BS
GB/T 699-1999
25
S25C 1025 ISO 630-1:1987
C25
C25E4
C25M2
C25
XC25
25 060A25
070A26

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!