Grade X2CrNiN23-4
European Standard Steel Grade 1.4362
Corresponding Standard EN 10088-3-2005
Stainless steels--Part 3:Techincal delivery conditions for semi-finished products,bar,rods and sections for general purposes
Classification Duplex Stainless Steel
X2CrNiN23-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N
Minimum Value - - - - - 22 3.5 0.1 0.1 0.05
Maximum Value 0.03 1 2 0.035 0.015 24 5.5 0.6 0.6 0.2
① Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
1 Approximate Comparison Table Austenitic-Ferritic Stainless Steel
China United States International Organization for Standardization European Standard
GB ISC ASTM UNS ISO EN Numerical Grade
022Cr23Ni4MoCuN S23043 2304 S32304 X2CrNiN 23-4 X2CrNiN 23-4 1.4362
2 Approximate Comparison Table Austenitic-Ferritic Stainless Steel
United States France European Standard Russia Sweden
UNS NF EN/NF EN Numerical Grade GOST SS
S32304 Z3CN23-04Az X2CrNiN23-4 1.4362 03KH23N6 2327

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!