Grade 16Mo3
European Standard Steel Grade 1.5415
Corresponding Standard EN 10217-5-2019
Part 5: Submerged Arc Welded Non- Alloy and Alloy Steel Tubes with Specified Elevated Temperature Properties
Classification Alloy Steel
16Mo3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo Al
Minimum Value 0.12 - 0.4 - - - - - 0.25 -
Maximum Value 0.2 0.35 0.9 0.025 0.02 0.3 0.3 0.3 0.35 0.04
※ In order to facilitate subsequent forming operations, an agreed maximum copper content lower than indicated and an agreed specified maximum tin content shall apply
ⓐ For wall thickness ≥ 30 mm the carbon content may be increased by 0,02 % for cast and product analysis.
16Mo3 Mechanical Properties
wall thickness
T
mm
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
T≤16 450~600 or ReH
≥280
≥22(l)
≥20(t)
20°C:
≥40(l);≥27(t)
16<T≤40 450~600 or ReH
≥270
≥22(l)
≥20(t)
20°C:
≥40(l);≥27(t)
• l = longitudinal; t = transverse
1 Approximate Comparison Table Pressure-Bearing Flat Steel
International Organization for Standardization European Standard
ISO EN Numerical Grade
16Mo3 16Mo3 1.5415
2 Approximate Comparison Table Structural Alloy Steel
Japan United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade SS BS EN/BS
STBA12 A204Gr.A
A204Gr.B
F26
P26
TS26
15Mo3
16Mo3
15D3 16Mo3 1.5415 2912 1503-243B
240
243
3 Approximate Comparison Table Seamless Steel Tubes and Pipes for High Pressure Boiler
China European Standard
GB ISC EN
15MoG A65158 16Mo3

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!