Grade 16NiCrS4
European Standard Steel Grade 1.5715
Corresponding Standard EN 10084-2008
Case Hardening Steels - Technical Delivery Conditions
Classification Alloy Steel
Properties Carburizing Ability
16NiCrS4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.13 - 0.7 - 0.02 0.6 0.8
Maximum Value 0.19 0.4 1 0.025 0.04 1 1.1
16NiCrS4 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Semifinished products, bars Processed to a Certain Shearability (+S) ≤255
All product shapes Soft Annealing (+A) ≤217
Bar, wire, flat steel, forging Processed to a Certain Hardness (+TH) 166~217
Bar, forging Processed to Ferrite-Perlite Structure (+FP) 156~207
1 Approximate Comparison Table Structural Alloy Steel
International Organization for Standardization European Standard
ISO EN Numerical Grade
16NiCrS4 16NiCrS4 1.5715
2 Approximate Comparison Table Alloy Surface Hardening Steel
United States European Standard Sweden
ASTM/AISI EN Numerical Grade SS
3115 16NiCrS4 1.5715 SS2511

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!