Grade 22CrMoS 3-5
European Standard Steel Grade 1.7333
Corresponding Standard EN 10084-2008
Case Hardening Steels - Technical Delivery Conditions
Classification Alloy Steel
Properties Carburizing Ability
22CrMoS 3-5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo
Minimum Value 0.19 - 0.7 - 0.02 0.7 0.4
Maximum Value 0.24 0.4 1 0.025 0.04 1 0.5
22CrMoS 3-5 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Rough, Bar Steel Processed to a Certain Shearability (+S) ≤255
All product shapes Soft Annealing (+A) ≤217
Bars, wire, plates, forgings; d≤150 Processed to a Certain Hardness (+TH) 170~217
Bar stock, plate, forgings; d≤60 Processed to Ferrite-Perlite Structure (+FP) 152~201
1 Approximate Comparison Table Hardenability Guaranteed Structural Steel
China Taiwan, China Japan South Korea International Organization for Standardization Germany France European Standard Russia United Kingdom
GB ISC CNS JIS KS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
22CrMoH A30225 SCM822H SCM822H SCM822H 22CrMoS3-5 20CrMo5 1.7264 (40CD4) 22CrMoS3-5 1.7333 ≈20ХМ 20CrMo5
2 Approximate Comparison Table Structural Alloy Steel
Germany European Standard
DIN EN/DIN EN Numerical Grade
22CrMoS3-5 22CrMoS3-5 1.7333

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!