Grade C20
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Carbon Steel
Properties Carburizing Ability
C20 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.17 0.1 0.3 - -
Maximum Value 0.23 0.4 0.6 0.045 0.045
◎ Steels with machinability which has been improved either by the addition of lead or by higher sulfur levels up to about 0.100 % (m/m) S (including controlled sulfide morphology) may be available on request.
C20 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤5 TC ≥580 ≥460 ≥5
5<t≤10 TC ≥540 ≥415 ≥5
10<t≤16 TC ≥490 ≥370 ≥7
16<t≤25 TC ≥470 ≥340 ≥8
25<t≤40 TC ≥450 ≥320 ≥9
40<t≤100 TC ≥400 ≥210 ≥11
t≤100 TC+TA,
P+TA
or
G+TA
≥156
t≤100 TC+TN,
P+TN
or
G+TN
≥400 ≥210 ≥27
100<t≤250 TC
or
TC+TN,
P+TN
or
G+TN
Be agreed Be agreed Be agreed
t≤250 TC+TQ+TT,
P+TQ+TT
or
G+TQ+TT
Be agreed Be agreed Be agreed
100<t≤250 TC+TA,
P+TA
or
G+TA
Be agreed
C20 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!