Grade C30
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Carbon Steel
Properties Carburizing Ability
C30 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.27 0.1 0.5 - -
Maximum Value 0.34 0.4 0.8 0.045 0.045
◎ Steels with machinability which has been improved either by the addition of lead or by higher sulfur levels up to about 0.100 % (m/m) S (including controlled sulfide morphology) may be available on request.
C30 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤5 TC ≥650 ≥520 ≥5
5<t≤10 TC ≥610 ≥475 ≥6
10<t≤16 TC ≥570 ≥430 ≥7
16<t≤25 TC ≥550 ≥395 ≥8
25<t≤40 TC ≥520 ≥370 ≥9
40<t≤100 TC ≥480 ≥250 ≥9
t≤100 TC+TA,
P+TA
or
G+TA
≥170
t≤16 TC+TN,
P+TN
or
G+TN
≥510 ≥260 ≥20
16<t≤100 TC+TN,
P+TN
or
G+TN
≥480 ≥250 ≥21
100<t≤250 TC+TN,
P+TN
or
G+TN
≥460 ≥230 ≥21
t≤16 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
600~750 ≥400 ≥18
16<t≤40 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
550~700 ≥350 ≥20
40<t≤100 TC+TQ+TT,
P+TQ+TT
or
G+TQ+TT
500~650® ≥300® ≥21®
100<t≤250 TC Be agreed Be agreed Be agreed
100<t≤250 TC+TA,
P+TA
or
G+TA
Be agreed
100<t≤250 TC+TQ+TT,
P+TQ+TT
or
G+TQ+TT
Be agreed Be agreed Be agreed

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!