Grade C25M2
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Carbon Steel
Properties Carburizing Ability
C25M2 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.22 0.1 0.4 - 0.02
Maximum Value 0.29 0.4 0.7 0.035 0.04
◎ Steels with machinability which has been improved either by the addition of lead or by higher sulfur levels up to about 0.100 % (m/m) S (including controlled sulfide morphology) may be available on request.
C25M2 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
t≤5 TC ≥610 ≥490 ≥5
5<t≤10 TC ≥580 ≥445 ≥6
10<t≤16 TC ≥530 ≥400 ≥7
16<t≤25 TC ≥510 ≥370 ≥8
25<t≤40 TC ≥490 ≥350 ≥9
40<t≤100 TC ≥440 ≥230 ≥10
t≤100 TC+TA,
P+TA
or
G+TA
≥156
t≤16 TC+TN,
P+TN
or
G+TN
≥470 ≥260 ≥22
16<t≤100
TC+TN,
P+TN
or
G+TN
≥440 ≥230 ≥23
t≤16 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
550~700 ≥370 ≥19 KU: ≥35
KV: ≥45
16<t≤40 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
500~650 ≥320 ≥21 KU: ≥35
KV: ≥45
40<t≤250 TC+TQ+TT,
P+TQ+TT
or
G+TQ+TT
Be agreed Be agreed Be agreed Be agreed
100<t≤250 TC
or
TC+TN,
P+TN
or
G+TN
Be agreed Be agreed Be agreed
t≤250 TC+TA,
P+TA
or
G+TA
Be agreed
C25M2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!