Grade C45
Corresponding Standard JIS G 7105-2000
Heat-Treatable Steels, Alloy Steels and Free-Cutting Steels — Part 18 : Bright Products Of Unalloyed and Low Alloy Steels
Classification Carbon Steel
Properties Carburizing Ability
C45 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.42 0.1 0.5 - -
Maximum Value 0.5 0.4 0.8 0.045 0.045
◎ Steels with machinability which has been improved either by the addition of lead or by higher sulfur levels up to about 0.100 % (m/m) S (including controlled sulfide morphology) may be available on request.
C45 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤5 TC ≥750 ≥610 ≥4
5<t≤10 TC ≥730 ≥560 ≥5
10<t≤16 TC ≥690 ≥520 ≥5
16<t≤25 TC ≥660 ≥475 ≥6
25<t≤40 TC ≥640 ≥450 ≥7
40<t≤100 TC ≥580 ≥305 ≥8
t≤100 TC+TA,
P+TA
or
G+TA
≥207
t≤16 TC+TN,
P+TN
or
G+TN
≥620 ≥340 ≥14
16<t≤100 TC+TN,
P+TN
or
G+TN
≥580 ≥305 ≥16
100<t≤250 TC+TN,
P+TN
or
G+TN
≥560 ≥275 ≥16
t≤16 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
700~850 ≥490 ≥14
16<t≤40 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
650~800 ≥430 ≥16
40<t≤100 TC+TQ+TT℗,
P+TQ+TT
or
G+TQ+TT
630~780 ≥370 ≥17
100<t≤250 TC Be agreed Be agreed Be agreed
100<t≤250 TC+TA,
P+TA
or
G+TA
Be agreed
100<t≤250 TC+TQ+TT,
P+TQ+TT
or
G+TQ+TT
Be agreed Be agreed Be agreed

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!